磨料种类和硬度与表面粗糙度及磨料粒度的关系
磨料种类和硬度
粗糙度值/μm
13
25
38
51
63
76
102
硅砂莫氏5~6
80/120
(0.18~0.125
30/50
(0.3~0.6)
20/40
(0.425~0.8)
16/30
(0.6~1.18)
12/25
(0.71~1.7)
10/20
(0.85~2.00)
8/16
(1.18~2.36)
矿砂莫氏7
90
80
(0.18)
55
金刚砂莫氏7~8
100
(0.15)
80
(0.13)
60
(0.25)
40
(0.425)
36
(0.5)
24
(0.71)
16
(1.18)
燧石莫氏 6.5~7
30/60
(0.253~0.6)
20/50
(0.30~0.85)
16/35
(0.5~1.18)
10/30
(0.6~2.00)
8/25
(0.71~2.36)
6/20
(0.85~3.35)
煤渣莫氏7
50/100
(0.15~0.3)
40/70
(0.21~0.42)
30/60
(0.25~0.6)
20/40
(0.425~0.8)
16/30
(0.6~1.18)
12/20
(0.82~1.7)
铜/镍炉渣莫氏7~7.5
70/100
(0.15~0.2)
60/80
(0.18~0.25)
40/80
(0.18~0.42)
30/50
(0.3~0.6)
20/40
(0.425~0.8)
16/30
(0.6~1.18)
氧化铝莫氏8
从经济性考虑,氧化铝磨料只能用于喷丸间或喷丸箱,回收再利用
120
(0.125)
80
(0.18)
50
(0.3)
40
(0.425)
36
(0.5)
24
(0.71)
16
(1.18)
碳化硅莫氏8
从经济性考虑,碳化硅磨料只能用于喷丸间或喷丸箱,回收再利用
150
(0.1)
100
(0.15)
80
(0.18)
50
(0.3)
40
(0.425)
36
(0.5)
30
(0.6)
核桃壳莫氏8
核桃壳磨料一般只用于清理或去毛刺,不以粗糙度为目的,需回收再利用
35/60
(0.25~0.5)
14/30
(0.6~1.4)
6/10
(2~3.35)
塑料磨料莫氏3~4
塑料磨料通常用于清除旧漆皮,清理硬度不高的表面,不以粗糙度过目的,需回收再利用
粒度有:12/16(1.18~1.7), 16/20(0.85~1.18), 20/30(0.6~0.85), 30/40(0.43~0.6), 40/60(0.25~0.425), 60/80(0.18~0.25),
玉米棒磨料莫氏4.5
用于清除电机、砖石、木材等表面,可产生轻微的粗糙度。
粒度:6/10(2~3.35), 8/12(1.7~2.36), 12/20(0.85~1.7), 14/30(0.63~1.4), 18/40(0.425~1.0), 35/60(0.25~0.5),40/100(0.15~0.425)
钢砂,铁砂rc40~68
只用于喷丸间和喷丸箱,回收再利用,只要使用恰当,经济性
g-200 g-120 g-80 g-50 g-40 g-25 g-16
(0.075) (0.125) (0.18) (0.3) (0.425) (0.71) (1.18)
塑料磨料莫氏5~6
用于表面褪光处理,粒度:粗级20/30(0.6~0.85)到细级170/325(约0.09)
钢丸,铁丸rc40~68
通常用于抛丸清理,仅列出粒度范围,选用时要考虑其他因素
粒度范围:s780~s70(0.18~2.0)